Para adicionar um pouco à pergunta de Pavel nos comentários de Ecnerwals, responda:
Stainless steel structures in swimming pools are known to be prone to SCC. The use of standard austenitic stainless steels like 304 and 316 is forbidden in this application. The best steels to use for this purpose are the high nickel austenitic steels such as the 6% Mo grades. However, in some cases, duplex steels such as 2205 (1.4462) and the superduplex grades can be considered.
Stress Corrosion Cracking (SCC) is a form of corrosion which occurs with a particular combination of factors:
Tensile stress
Corrosive environment
Sufficiently high temperature
Normally 50 deg C but can occur at lower temperatures around 25 deg C in specific environments, notably swimming pools.
Unfortunately, the standard austenitic steels like 304 (1.4301) and 316 (1.4401) are the most susceptible to SCC
fonte
Claro, as piscinas contêm cloro e geralmente têm uma temperatura e outras coisas mais altas, mas é melhor prevenir do que remediar.
Como o OP pediu o aço mais adequado, eu gostaria de sugerir Aço inoxidável Duplex 1.4462. É aço não corrosivo, com excelentes propriedades.
Propriedades:
- resistência à corrosão particularmente alta,
- muito boas propriedades mecânicas,
- adequado para uso em temperaturas de -100 ° C a 250 ° C,
- médio bom perdoável, bom soldável,
- polida, magnetizável
Aplicação:
- indústria da construção
- indústria química e petroquímica
- indústria alimentícia
- mar
- construção naval
- engenharia de máquinas